Polyester Viscose Fabrics siamna atana hmanraw pawimawh ber berte

Jun 17, 2025

Message pakhat dah la .

1. Raw Material hmanga tihfai hmasak
• Polyester Chip Drying: Polyester has extremely low hygroscopicity, but excessive moisture content (>0.02%) chu awlsam takin a hydrolyze thei a, spinning laiin a chhe thei bawk. Drying hi vacuum drum dryer-ah darkar 4-6 chhung 120-140 degree-ah tih a ni a, chu chuan moisture content chu 50 ppm aia hniam a ni.

• Viscose Fiber siam dan: Viscose hian aging, yellowing leh dissolution a paltlang a, spinning solution (alkali cellulose awmna viscous solution) a siam a ni. Chumi hnuah filtration leh degassing hmangin bawlhhlawh leh bubble te chu paih chhuah a ni a, chu chuan spinnability a ti thei a ni. Viscose fiber hi a tlangpuiin staple fiber (viscose staple fiber ang chi) angin an inhmeh a, a sei zawng chu 38-51 mm niin a fineness chu 1.67-2.22 dtex a ni.

 

2. Spinning Process tih dan tur

Blended yarn hi kawng hnih hmanga siam a ni ber a:

• Ring Spinning: Polyester staple fiber leh viscose staple fiber te chu a inang tlangin an inhmeh (manual premixing emaw disc blender hmangin). Chumi hnuah chuan blended yarn chu hawn, carding, drawing, roving leh spinning hmangin an process leh thin. Hetiang method hian fiber blending uniform tak a ti thei a, puan pangngai tan pawh a tha a, mahse production efficiency a hniam zawk thung.

• Siro Spinning/Compact Spinning Optimization: Rovings pahnih (polyester yarn pakhat leh viscose yarn pakhat) chawm a, twisting atan an inzawmkhawm hian yarn chakna leh yarn uniformity a ti tha a, chutih rualin hairiness a ti tlem a, high-end fabrics atan a tha zawk.

 

3. Puan siam dan (Weaving Process).

Blended yarn hi target fabric chi hrang hrang a zirin woven emaw knitted emaw theih a ni:

• Woven Fabrics: Woven fabrics-ah hian plain, twill emaw satin weaves emaw hman a ni a, warp leh weft yarn pahnih hi polyester/viscose blend (eg, 65/35 ratio) a ni. Weaving lai hian viscose fibers-a static electricity (chu chu waxing emaw workshop-a humidity 60-70% thlenga tihpun emaw hmanga tihziaawm theih) ngaihven tur a ni.

• Knitted fabrics: Weft-knitted circular emaw flat knitting machine, jersey leh rib ang chiah-a siam tlangpui a ni a, viscose fibers hian a softness hmangin a hatu fit a tichak a, polyester fibers erawh chuan loop stability a tichiang thung.

 

4. Key Finishing Step hrang hrang
• Desizing leh Scouring: Fabric-ah hian sizing (woven fabrics tan) a awm chuan desizing enzyme emaw alkali agents hmangin natural impurities leh spinning auxiliary te paih chhuah a ni. Hetih lai hian viscose fibers tan alkali concentration (<=5g/L) control tur a ni a, chutiang chuan a chhiat lutuk loh nan.

• Softening leh Setting: Padding softeners (silicones ang chi) hi kut feel tihchak nan hman a ni a, high-temperature setting (180-200℃for 20-30 seconds) erawh chuan polyester dimensional stability a stabilize a, viscose fiber a shrinkage lutuk tur a veng bawk (viscose atana heat shrinkage rate chu a tlem berah a ni 5-8% a ni a, chu chu polyester tan chauh a ni 0.4-0.8%) a ni.

• Dyeing process : Polyester hian temperature sang leh pressure sang disperse dyeing (130℃vel) a mamawh avangin, viscose fiber erawh chu room temperature leh normal pressure (60-80℃)-a reactive dyeing atan a tha a, two-bath method of "dying viscose first and then polyester" tih hi hman a ni tlangpui a, a nih loh leh process chu optimized through the "one-bath two-step method" (temperature hniam takah viscose thih hmasak a, temperature sang zawka polyester dye).

 

Inquiry thawn rawh .